Patent · US Active

Cold rolled steel sheet and method for producing same

US12180557B2 · kind B2 · utility

0Cited by
0References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 31, 2020
Grant dateDec 31, 2024
Priority date
Expiry dateJan 16, 2042

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/008
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention relates to a cold rolled steel sheet containing C: 0.15% or more and 0.40% or less, Si: 0.50% or more and 4.00% or less, Mn: 1.00% or more and 4.00% or less, and sol. Al: 0.001% or more and 2.000% or less, having a metallic structure consisting of 35 to 65 area % of ferrite phases, 35 to 65 area % of hard second phases, and 0 to 5 area % of remaining phases, wherein 60% or more of the ferrite phases are recrystallized ferrite phases, an average crystal grain size defined by 15° grain boundaries is 5.0 μm or less, a maximum connecting rate of the hard second phases is 10% or more, and a two-dimensional isoperimetric constant of the hard second phases is 0.20 or less.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.