Method of preparing biodegradable Zn—Mg—Bi zinc alloy
US12203152B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Dec 22, 2023 |
| Grant date | Jan 21, 2025 |
| Priority date | — |
| Expiry date | Dec 22, 2043 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22C30/06
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of preparing biodegradable Zn—Mg—Bi zinc alloy includes: melting magnesium under an inert atmosphere to obtain a magnesium melt; adding bismuth particles to the magnesium melt followed by reaction under stirring and heat preservation treatment to obtain a Mg—Bi alloy melt; allowing the Mg—Bi alloy melt to stand in a furnace; subjecting the Mg—Bi alloy melt to refining, slagging-off, casting and demoulding to obtain Mg-50 wt. % Bi alloy ingot; melting zinc to obtain a zinc melt; adding the Mg-50 wt. % Bi alloy ingot and pure magnesium or pure bismuth followed by heating to a preset temperature, stirring and heat preservation to obtain a Zn—Mg—Bi alloy melt; allowing the Zn—Mg—Bi alloy melt to stand in a furnace followed by refining, slagging-off, casting and demoulding to obtain the biodegradable Zn—Mg—Bi zinc alloy.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.