Method for producing a rubber-plastic composite
US12247118B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Sep 1, 2020 |
| Grant date | Mar 11, 2025 |
| Priority date | — |
| Expiry date | Nov 13, 2041 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L2312/00
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
A method for producing a rubber-plastic composite, including the steps of (a) shaping an unvulcanized elastomer, (b) partially vulcanizing the shaped elastomer at a temperature of at least 140° C. up to a degree of vulcanization in the range from 10% to 40%, (c) cooling the partially vulcanized elastomer to a temperature of less than 100° C. within less than 20 minutes, (d) overmolding the partially vulcanized elastomer with a plastic, and (e) heat treating the partially vulcanized elastomer overmolded with a plastic at a temperature in the range from 100° C. to 170° C. for a duration of from 5 minutes to 5 hours to complete the vulcanization and form a rubber-plastic composite. The method further relates to a rubber-plastic composite obtainable by the method according to the invention and also to a shoe comprising the rubber-plastic composite obtainable by the method according to the invention.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.