Tube-drawable glass, method for the production and use

US12252439B2 · kind B2 · utility

0Cited by
2References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 18, 2020
Grant dateMar 18, 2025
Priority date
Expiry dateJan 16, 2042

Classification

  • Technology area (CPC G)Physics
  • CPC primaryG02B5/226
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A glass has a maximum crystallization rate (KGmax) of at most 0.20 μm/min in a temperature range of 700° C. to 1250° C. and a hydrolytic stability according to a hydrolytic class 1 HGA1 according to ISO 720:1985. In the case of a sample thickness of 2 mm of the glass, a ratio of a minimum transmittance in a wavelength range of 850 nm to 950 nm to a maximum transmittance in a wavelength range of 250 nm to 700 nm is in a range of 1.9:1 to 15:1.