Patent · US Active

Rapid and comprehensive method for evaluating pitting resistance of stainless steel pipe welds

US12259313B1 · kind B1 · utility

0Cited by
0References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 4, 2024
Grant dateMar 25, 2025
Priority date
Expiry dateSep 4, 2044

Classification

  • Technology area (CPC G)Physics
  • CPC primaryG01N17/006
  • WIPO fieldMeasurement
  • WIPO sectorInstruments

Abstract

The disclosure relates to a rapid and comprehensive method for evaluating pitting resistance of stainless steel pipe welds. Weld samples are collected from different positions of one or more welds on the stainless steel pipe to obtain the surface oxide inclusion density and critical pitting temperature of each weld sample, the surface oxidation inclusion density is taken as an independent variable and the critical pitting temperature is taken as a dependent variable to obtain a fitting function formula between the surface oxidation inclusion density and the critical pitting temperature. The surface oxide inclusion density obtained by adopting the same welding process on the stainless steel pipe to be tested is substituted into the fitting function formula to obtain a standard critical pitting temperature of the weld to be tested. The pitting resistance of the weld of the stainless steel pipe to be tested can be evaluated rapidly, accurately, and comprehensively.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.