Abstract

A method for producing a molten steel may provide: solid-state direct reduced iron containing 3.0% by mass or more of SiO2 and Al2O3 in total and 1.0% by mass or more of carbon, a ratio of a metallic iron to a total iron content contained in the solid-state direct reduced iron being 90% by mass or more, and an excess carbon content Cx to the carbon contained in the solid-state direct reduced iron being 0.2% by mass or more. Such methods may include: a slag separation including heating the solid-state direct reduced iron and melting it in an electric furnace without introducing oxygen to separate into a molten steel and a slag, and continuously discharging the slag, and a decarburization including blowing, in the electric furnace, a total amount of oxygen introduced into the electric furnace to the molten steel to decarburize the molten steel after the slag separation.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.