Patent · US Active

Method for producing molten steel

US12281365B2 · kind B2 · utility

0Cited by
2References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 11, 2020
Grant dateApr 22, 2025
Priority date
Expiry dateJul 11, 2041

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P10/20
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method includes, in a first furnace, melting 40% to 95% by mass of a solid-state direct reduced iron, and separating a molten pig iron having a carbon content of 2.0% to 5.0% by mass and a temperature of 1350 to 1550° C. and a slag having a basicity of 1.0 to 1.4. In a second furnace, a remainder of the solid-state direct reduced iron is melted together with the molten pig iron separated in the first furnace to form a molten material, and oxygen is blown onto the molten material to decarburize into a molten steel. The solid-state direct reduced iron includes 3.0% by mass or more of SiO2 and Al2O3 in total and 1.0% by mass or more of carbon. A ratio of a metallic iron to a total iron content contained in the solid-state direct reduced iron is 90% by mass or more.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.