Press hardening method

US12281366B2 · kind B2 · utility

0Cited by
1References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 20, 2020
Grant dateApr 22, 2025
Priority date
Expiry dateDec 3, 2041

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/008
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A press hardening method includes the following steps: A. the provision of a steel sheet for heat treatment, precoated with a zinc- or aluminum-based pre-coating for anti-corrosion purpose, B. the deposition of a hydrogen barrier pre-coating over a thickness from 10 to 550 nm, C. the batch annealing of the precoated steel sheet in an inert atmosphere to obtain a pre-alloyed steel sheet, D. the cutting of the pre-alloyed steel sheet to obtain blank, E. the thermal treatment of the blank to obtain a fully austenitic microstructure in the steel, F. the transfer of the blank into a press tool, G. the hot-forming of the blank to obtain a part, H. the cooling of the part obtained at step G).

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.