Method for fabricating an environmental barrier coating on a ceramic matrix composite
US12304874B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Sep 21, 2023 |
| Grant date | May 20, 2025 |
| Priority date | — |
| Expiry date | Sep 21, 2043 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02T50/60
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of fabricating a coating includes providing a ceramic matrix composite that includes SiC fibers disposed in a SiC matrix, depositing a base slurry on the ceramic matrix composite, wherein the base slurry contains powders of a metal oxide, at least one of silicon carbide, silicon nitride, or free silicon, and barium-magnesium-aluminosilicate in a first carrier fluid, drying the deposited base slurry to produce a base green layer, depositing a transition slurry on the base green layer, wherein the transition slurry contains powders of a metal oxide, at least one of silicon carbide, silicon nitride, or free silicon, at least one of zirconium carbide, zirconium nitride, or zirconium oxide, and barium-magnesium-aluminosilicate in a second carrier fluid, drying the deposited transition slurry to produce a transition green layer, and forming a consolidated coating on the ceramic matrix composite by heating the base green layer and the at least one transition green layer to cause chemical reactions that convert the powders to metal-silicon-oxygen rich phase and metal-zirconium-oxygen rich phase.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.