Overlay welding material

US12318872B2 · kind B2 · utility

0Cited by
1References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 29, 2022
Grant dateJun 3, 2025
Priority date
Expiry dateMar 29, 2042

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E30/30
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A steek suitable for structural components used in contact with liquid lead or liquid lead alloys in nuclear reactors consisting of in weight % (wt. %): C 0.02-0.09; Si 0.1-1.6; Mn 1.5-3.0; Cr 9.0-12.0; Ni 10.0-16.8; Al 2.0-3.4; Ti 0.1-1.0; Nb≤0.5; V≤0.5; Ta≤1.5; Y≤0.5; Mo≤1.5; W≤1.5; Cu≤1.7; N≤0.06; Co≤1.0; B≤0.1; Zr≤0.5; Hf≤0.5; RE≤0.2; Ca≤0.1; Mg≤0.1; Bi≤0.1; SE≤0.1 and balance Fe apart from impurities, wherein the content of RE does not include the amount of Y but only the amount of the elements having an atomic numbers 21 and 57-71, wherein the steel fulfils one or more of the following requirements:

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.