TIG welding filler metal and method for producing weld joint using the same

US12383989B2 · kind B2 · utility

0Cited by
0References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 16, 2021
Grant dateAug 12, 2025
Priority date
Expiry dateDec 16, 2041

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB23K2103/04
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A TIG welding filler metal is provided that has a composition including, by mass %, C: 0.20 to 0.80%, Si: 0.15 to 0.90%, Mn: 15.0 to 30.0%, P: 0.030% or less, S: 0.030% or less, Cr: 6.0 to 15.0%, and N: 0.120% or less, the balance being Fe and incidental impurities. Where necessary, the filler metal may contain one or two selected from Ni and Mo, may further contain one, or two or more selected from V, Ti, and Nb, and may additionally contain one, or two or more selected from Cu, Al, Ca, and REM. This configuration reduces the occurrence of welding cracks during TIG welding, that is, realizes excellent hot crack resistance, and allows for easy production of a weld joint having high strength and excellent cryogenic impact toughness.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.