Lamination member and glass composition

US12410105B2 · kind B2 · utility

0Cited by
6References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 18, 2023
Grant dateSep 9, 2025
Priority date
Expiry dateMar 18, 2044

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2237/365
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention relates to a laminated member, including: a glass member having a linear transmittance at a wavelength of 850 nm of 80% or more; a bonding layer containing a resin and lying on the glass member; and a Si—SiC member lying on the bonding layer, in which the glass member includes predetermined amounts of SiO2, Al2O3, B2O3, and P2O5, the Si—SiC member has an average linear expansion coefficient α at 20 to 200° C. of 2.85 to 4.00 ppm/° C., and has an average linear expansion coefficient β at 20 to 200° C. of 1.50 to 5.00 ppm/° C., and the laminated member has an absolute value |α-β|, which is a value obtained by subtracting β from α, of 2.00 ppm/° C. or less.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.