Method of manufacturing a spheroidal reforming catalyst
US3943071A · kind A · utility
1Cited by
1References
9Claims
0Family size
Assignee
Inventor
Key dates
| Filing date | Oct 15, 1974 |
| Grant date | Mar 9, 1976 |
| Priority date | — |
| Expiry date | Oct 15, 1994 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB01J23/626
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
A method of manufacturing a high surface area, spheroidal reforming catalyst comprising a tin-promoted, alumina-supported platinum group metal. A soluble tin compound and a finely divided eta-alumina are combined with an acidic alumina hydrosol, and the mixture thereafter converted to spheroidal particles by the oil-drop method. The spheroidal particles are subsequently impregnated with a platinum group metal component.