Patent · US Expired

Boron-hardened tungsten facing alloy

US3947269A · kind A · utility

7Cited by
8References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 24, 1972
Grant dateMar 30, 1976
Priority date
Expiry dateAug 24, 1992

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/1284
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

This invention relates to an alloy useful as a hard facing material. The alloy comprises a matrix such as a nickel-chromium matrix containing a separate interstitially boron-hardened tungsten phase. The alloy is used as a facing or coating for a number of base materials, and in particular as a piston ring facing. The invention is also concerned with a method of making said alloy by utilizing a plasma jet spray technique.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.