Patent · US Expired

Size-graded quaternary batch for bonded basic refractory shapes

US3948671A · kind A · utility

3Cited by
3References
9Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 17, 1974
Grant dateApr 6, 1976
Priority date
Expiry dateJun 17, 1994

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B35/06
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A refractory of fused or dead-burned dolomitic grain bonded with fine magnesite. The dolomitic grain is divided into three coarse and intermediate particle size fractions in the batch, while the magnesite is alone in the fine fraction. The four particle fractions are separated by three discrete gaps in the size distribution of particles resulting in a burned refractory of high hot strength and corrosion resistance to furnace slags in basic oxygen furnaces. The width of each gap is at least equivalent to the gap created by removing, from a ground raw material batch with continuous particle size distribution, the raw material retained on one primary Tyler sieve after screening (sizing) the batch.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.