Patent · US Expired

Aluminum smelting temperature selection

US3951763A · kind A · utility

11Cited by
1References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 7, 1975
Grant dateApr 20, 1976
Priority date
Expiry dateMar 7, 1995

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC25C3/06
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

A process for producing aluminum in which alumina is decomposed electrolytically to aluminum metal in an electrolyte bath between an anode and a cathodic interface formed between aluminum metal and the electrolyte bath. The bath consists essentially of Al.sub.2 O.sub.3, NaF, and AlF.sub.3, and has a weight ratio NaF to AlF.sub.3 up to 1.1:1. During decomposition, the bath is maintained at an operating temperature greater than 40.degree.C above the cryolite liquidus temperature of the bath and effective for preventing bath crusting in interfacial areas between bath and aluminum metal.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.