Manufacture of homopolymers of 4-methylpentene-1
US3969335A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Feb 6, 1975 |
| Grant date | Jul 13, 1976 |
| Priority date | — |
| Expiry date | Feb 6, 1995 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S526/905
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Homopolymers of 4-methylpentene-1 are prepared by homopolymerization of 4-methylpentene-1 at a temperature above room temperature, in the presence of hydrogen and in contact with a Ziegler/Natta catalyst system. The polymerization is carried out at a relatively very high temperature and in the presence of an inert gas, the polymerization system being under a specific total pressure, while the partial pressures of the inert gas and the hydrogen have specific values. In this way, homopolymers having large crystalline fractions are obtained in high yields per unit of catalyst system per unit time.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.