Abstract
Method of preparation of an alloy comprising the steps of preparing a nickel-iron-chromium based alloy, placing the alloy in solution at temperatures between 925.degree.C and 1060.degree.C, followed by a quick cooling, aging the alloy at a first level of temperature and exposure time to obtain a precipitation of .gamma.' phase prior to a precipitation of a .gamma." phase and reducing the temperature to a second level of at least 700.degree.C.