"Composition for permanent magnets of the family ""rare earths-transition metals"" and process for producing such a magnet"

US4002508A · kind A · utility

4Cited by
3References
6Claims
0Family size

Assignee

Inventor

Key dates

Filing dateAug 14, 1975
Grant dateJan 11, 1977
Priority date
Expiry dateAug 14, 1995

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01F1/055
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention relates to a composition for permanent magnets of the family "rare earths-transition metals" wherein in a structure of the SmCo.sub.5 type, 2 to 15% of the cobalt atoms are replaced by nickel. This can be applied to the production by the sintered powder technique of permanent magnets having a particularly high intrinsic coercivity.