Colloidal polysulfone electrodeposition compositions
US4003812A · kind A · utility
7Cited by
4References
9Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Apr 15, 1975 |
| Grant date | Jan 18, 1977 |
| Priority date | — |
| Expiry date | Apr 15, 1995 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31678
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
A conducting, non-aqueous, colloidal, polysulfone electrodeposition composition is made by mixing: (1) 1 part polysulfone polymer and 20-37 parts non-aqueous, organic, aprotic solvent for the polysulfone polymer with (2) 0.8-1.2 parts of a nitrogen containing base, to form a polysulfone polymer solution, which is added to (3) 25-150 parts of a non-aqueous, non-solvent for the polysulfone polymer, which is miscible with the aprotic solvent.