Thermostable polyester
US4006120A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 5, 1974 |
| Grant date | Feb 1, 1977 |
| Priority date | — |
| Expiry date | Jun 5, 1994 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G63/193
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A process for the preparation of a thermostable polyester which is insoluble in tetrachloroethane and consists of about 40 to 200 units, said polyester having units of the formula ##STR1## combined with units of the formula ##STR2## wherein Ph is ##STR3## AND BOTH R radicals are methyl on some units and both R radicals are phenyl on the balance of the units, said methyl units comprising 5-30 mole percent of the total R-containing units which comprises heating and condensing in the absence of a catalyst 4,4'-dihydroxytetraphenylmethane having a melting point of at least 295.degree. C together with 2,2-bis-(4-hydroxyphenyl)-propane and terephthalic or isophthalic acid dichloride until there is prepared said polyester which is insoluble in tetrachlorethane.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.