Abstract
A method of compounding graphitizable compositions and improving the dispersion of filler particles and binder which comprises introducing the carbon filler into a hot-shear mixer, adding from about 25 to about 70 pph of water, adding from about 1/4 to about 5 pph of a dispersant, mixing for about 1/2 hour at a temperature at least above the boiling point of water (100.degree.), adding a binder, and mixing for about an additional one hour at a temperature above the melting point of the binder.