Process for obtaining a polyol-containing homogeneous liquid composition useful for the production of rigid polyurethane foam from a rigid polyurethane foam
US4014809A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Dec 19, 1975 |
| Grant date | Mar 29, 1977 |
| Priority date | — |
| Expiry date | Dec 19, 1995 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02W30/62
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
A process for obtaining a polyol-containing homogeneous liquid composition, which can be directly reused as a polyol component for the production of rigid polyurethane foam, from a rigid polyurethane foam, which comprises treating said foam at a temperature of from 150.degree. to 220.degree. C in the presence of a mixture of (a) an aliphatic diol having 4-7 carbon atoms and having a boiling point higher than 160.degree. C and (b) a monoalkanolamine having 2 to 8 carbon atoms, the amount of said monoalkanolamine (b) present in said mixture being within the range of from 1 to 20 percent by weight.