Abstract
In the rolling mill the temperature of the product is reduced to between Ac.sub.3 and Ac.sub.3 + 150.degree. C before it enters the finishing stands. The product emerging from the finishing stands is quenched to provide a surface layer of martensite and/or bainite. Subsequently the heat of the core of the product is allowed to raise the temperature of the surface layer to between 450.degree. and 750.degree. C, so that the quenched layer is tempered.