Patent · US Expired

Polytetramethylene ether urethane cured with 2,2'-diaminodiphenyl disulphide

US4017464A · kind A · utility

7Cited by
2References
2Claims
0Family size

Assignee

Inventor

Key dates

Filing dateFeb 5, 1976
Grant dateApr 12, 1977
Priority date
Expiry dateFeb 5, 1996

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08G18/4854
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Polytetramethylene ether urethane having improved physical properties is produced by reacting polytetramethylene ether polyol with a toluene diisocyanate containing at least 50 percent 2,4 isomer, reacting at a temperature no greater than about 40.degree. C. to produce a prepolymer and curing the prepolymer with 2,2'-dithio dianiline having the formula ##STR1## at a temperature of 105.degree. C.