A method for improving the strength of wire or strip having a composition which consists essentially of an austenitic metal alloy selected from the group consisting of stainless steel alloys of the AISI 200 and 300 series and non-stainless steel alloys containing iron, manganese, chromium, and carbon, said alloy having an Md temperature of no higher than about 100.degree. C and an Ms temperature of no higher than about minus 100.degree. C comprising the following step: PA1 Stretching the wire or strip uniaxially at a strain of at least about 10 percent and at a temperature no higher than about minus 75.degree. C in such a manner that the wire or strip has a martensite phase of at least about 50 percent by volume and an austenite phase of at least about 10 percent by volume.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.