Process for the conversion of pitch into crystalloidal pitch

US4042486A · kind A · utility

20Cited by
2References
22Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 10, 1976
Grant dateAug 16, 1977
Priority date
Expiry dateMar 10, 1996

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B35/528
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Crystalloidal pitch is obtained by subjecting solid pitch particles measuring not more than 5 mm in cross-sectional equivalent diameter to a treatment to prevent cohesion and subsequently bringing the cohesion-proof solid pitch particles into contact with a non-oxidative gas at temperatures of from 350.degree. C to 550.degree. C while maintaining a gas flow rate sufficient to provide a suspension wherein the gas constitutes at least 30% by volume. The crystalloid pitch is useful as a precursor for various carbon products.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.