Amorphous alloys with improved resistance to embrittlement upon heat treatment
US4052201A · kind A · utility
31Cited by
3References
5Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jun 26, 1975 |
| Grant date | Oct 4, 1977 |
| Priority date | — |
| Expiry date | Jun 26, 1995 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22C45/008
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
An improvement in resistance to embrittlement upon heat treatment of amorphous metal alloys containing iron, nickel, cobalt and/or chromium in the temperature range of about 200.degree. to 350.degree. C is achieved by including boron or boron plus at least one metalloid element of carbon, silicon and aluminum in a total amount of about 15 to 25 atom percent of the alloy composition.