Abstract

This invention relates to a super rapid hardening mixture comprising PA1 A. a super rapid hardening cement in which 11CaO.7Al.sub.2 O.sub.3. CaZ (X is a halogen atom), 3CaO.SiO.sub.2 and CaSO.sub.4 are present as indespensable components; PA1 B. at least one short range strength accelerator selected from the group consisting of a calcium aluminate material, a lime material, an amine and an ethylene glycol material and calcium sulfate hemihydrate; PA1 C. at least one emulsion selected from the group consisting of a bituminous emulsion, a rubber latex and a resin emulsion; PA1 D. from 12 to 50 weight percent of water in the total mixture.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.