Polyurethane composition having improved tear strength and process for preparation thereof
US4062825A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Oct 23, 1975 |
| Grant date | Dec 13, 1977 |
| Priority date | — |
| Expiry date | Oct 23, 1995 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH04L67/1097
- WIPO fieldComputer technology
- WIPO sectorElectrical engineering
Abstract
A polyurethane composition having high tear strength has been produced by mixing homogeneously 20 to 50 parts by weight of finely divided acidic silica particles, 100 parts by weight of isocyanate-terminated prepolymer and appropriate parts of curative, and curing the mixture in a manner well known in the prior art, where the ratio (l/d) of average chain distance (l) between adjacent crosslinking points of the cured polyurethane chains to average size (d) of finely divided silica particles is in the range of from 2.5 to 20.