Method of making fibrous alkali titanates
US4064224A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jan 28, 1976 |
| Grant date | Dec 20, 1977 |
| Priority date | — |
| Expiry date | Jan 28, 1996 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01P2006/60
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of making fibrous alkali titanates comprising the steps of preparing a mixture including a titanium compound and an alkali metal compound in a molar ratio of 1.0 to 8.0 in terms of TiO.sub.2 :M.sub.2 O (M: Na, K, Rb, Cs), heating said mixture at a temperature of 1200.degree. to 1600.degree. C to the molten (liquid) phase, cooling the thus heated mixture to room temperature , and washing the thus treated product. This method is advantageous because fibrous alkali titanates of large ratio of length to diameter can be easily produced in high yield.