Dehydrogenation of saturated hydrocarbons
US4070413A · kind A · utility
27Cited by
3References
11Claims
0Family size
Assignee
Inventor
Key dates
| Filing date | Oct 28, 1976 |
| Grant date | Jan 24, 1978 |
| Priority date | — |
| Expiry date | Oct 28, 1996 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC07C5/3337
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
Paraffinic hydrocarbons are dehydrogenated in contact with a catalytic composite comprising from about 0.01 to about 2.0 wt. % Group VIII metal and from about 0.01 to about 0.1 wt. % lithium impregnated on an alumina support, said alumina having been hydrothermally treated in steam at a temperature of from about 800.degree. to about 1200.degree. C.