Process for the hydrolysis of titanyl sulphate solutions
US4098869A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Oct 4, 1977 |
| Grant date | Jul 4, 1978 |
| Priority date | — |
| Expiry date | Oct 4, 1997 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01P2006/60
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Hydrolysis of a titanyl sulphate solution is carried out according to the autonucleation method of gradually adding the solution to a body of water at a substantially constant rate over 10-20 minutes, in such a way as to obtain an ionic concentration after one minute of feeding of from 75 to 105 g/l, the concentration of sulphuric acid in the final hydrolysis solution being regulated to a value of from 310 to 330 g/l by adding water from the commencement of clouding of the hydrolysis solution up to the end of hydrolysis.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.