Recovery of lithium from brines
US4116856A · kind A · utility
57Cited by
4References
9Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jul 5, 1977 |
| Grant date | Sep 26, 1978 |
| Priority date | — |
| Expiry date | Jul 5, 1997 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01F7/78
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
An anion exchange resin, containing Al(OH).sub.3 suspended therein, is reacted with aq. LiOH to form microcrystalline LiOH.2Al(OH).sub.3 which is then reacted with a halogen acid or halide salt to form microcrystalline LiX.2Al(OH).sub.3. The resin, after having a portion of the LiX eluted by using an aqueous wash, is used to recover Li.sup.+ values from aqueous brines.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.