Production of coated building components
US4117197A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Sep 7, 1976 |
| Grant date | Sep 26, 1978 |
| Priority date | — |
| Expiry date | Sep 7, 1996 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31652
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
In the production of a coated building component comprising the steps of mixing an inorganic binder, water and aggregate to produce a workable mass, molding said mass into a preformed component, applying to the preformed component an aqueous paste containing a metal oxide and at least one of waterglass and a phosphate to form a coating and allowing the coating to harden, the improvement which comprises applying about 190 to 400 g of the paste per square meter of surface to be coated, the application being effected in the presence of at least about 0.5% by weight of the inorganic binder or, in the case of lime-sand bricks, by weight of the binder plus aggregate, of a water soluble inorganic salt which converts the aqueous paste into a gel-like non-flowing form. The inorganic salt can be included in the workable mass from which the preformed component is molded or it may be present in a preliminary layer, along with inorganic binder, which is applied to the preformed component in a thickness of about 1 to 50 mm prior to application of the aqueous paste.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.