The present invention primarily comprises an improvement upon the method for producing photosensitive colored glasses or polychromatic glasses utilizing two sequences of exposure to high energy or actinic radiation followed by heat treatment. The invention contemplates replacing the second exposure/heat treatment step with a heat treatment conducted in a reducing atmosphere at a temperature of at least 350.degree. C., but below the strain point of the glass. The resultant articles can be particularly useful in ophthalmic applications.