Patent · US Expired

High-strength iron-molybdenum-nickel-phosphorus containing sintered alloy

US4128420A · kind A · utility

11Cited by
8References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 17, 1977
Grant dateDec 5, 1978
Priority date
Expiry dateMar 17, 1997

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C33/0264
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

To provide an alloy having high strength, toughness, and which is highly resistant to impact loading, the alloy has the following composition (all percentages by weight): 2-4.5 Mo, more than 2.5 to less than 3.5% Ni, more than 0.3 to less than 0.6% P, the rest iron; preferably, 3% Mo, 3% Ni, 0.45% P and the rest iron are used.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.