Patent · US Expired

Process for preparing a halogenated aromatic polyester having a predetermined molecular weight by solution polymerization technique

US4132705A · kind A · utility

1Cited by
3References
37Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 28, 1977
Grant dateJan 2, 1979
Priority date
Expiry dateJul 28, 1997

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08G63/6824
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A process for preparing certain halogenated aromatic polyesters having a predetermined molecular weight is provided. Such polyesters are prepared by solution polymerization of an appropriate bisphenol and diacid halide wherein the diacid halide is added to a solution containing the bisphenol until the viscosity of the resulting polymer containing solution reaches a predetermined solution viscosity limit at which time the further addition of diacid halide is terminated. The solution viscosity limit is indicative of the attainment of said predetermined molecular weight. The identification of said solution viscosity limit is achieved by a feedback mechanism wherein the viscosity of the polymer containing solution is monitored or sensed during or after the addition of the diacid halide to the bisphenol containing solution.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.