Aluminum alloy products of high corrosion resistance and deformability
US4137102A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 29, 1976 |
| Grant date | Jan 30, 1979 |
| Priority date | — |
| Expiry date | Jun 29, 1996 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31678
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
In the fabrication of an exhaust system of an internal-combustion engine, a tube-bank heat exchanger, a ducted-plate solar collector, saline water reclamation plant and enameled kitchenware, the improvement which comprises the use of a wrought aluminum alloy consisting essentially of: PA1 0.8 to 2.2% by weight manganese, PA1 0.1 to 0.5% by weight zirconium, PA1 0 to 1.0% by weight iron, PA1 0 to 0.6% by weight silicon, PA1 0 to 0.5% by weight copper, PA1 0 to 0.1% by weight magnesium, Balance aluminum and unavoidable impurities.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.