Magnesium alloys
US4149882A · kind A · utility
5Cited by
2References
15Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Oct 25, 1977 |
| Grant date | Apr 17, 1979 |
| Priority date | — |
| Expiry date | Oct 25, 1997 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22C23/00
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Magnesium alloys having improved high-temperature properties, especially improved resistance to creep, contain from 1.25 to 3.0% silver, 0.5 to 2.5% of rare metals including at least 60% neodymium and from 2.5 to 7.0% thorium. Optimum properties are obtained by high-temperature solution treatment followed by aging at a lower temperature.