Coal deashing process having improved solvent recovery techniques

US4162956A · kind A · utility

6Cited by
9References
13Claims
0Family size

Assignee

Inventor

Key dates

Filing dateMar 20, 1978
Grant dateJul 31, 1979
Priority date
Expiry dateMar 20, 1998

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC10G1/006
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

An improved coal deashing process wherein coal is mixed with a coal liquefaction process solvent, solubilized and flashed to provide a prepared mixture and the prepared mixture is mixed with a deashing solvent to produce a feed mixture. Thereafter, the feed mixture is separated in a first separation zone into a first heavy fraction comprising insoluble coal products and a first light fraction comprising soluble coal products and solvents. The first light fraction is recovered and a second portion of the deashing solvent is mixed with the first light fraction prior to introduction into a second separation zone wherein an improved separation occurs to produce a second light fraction comprising the solvents and a second heavy fraction comprising the soluble coal products which is recovered. The second light fraction is withdrawn and separated in a third separation zone into a third heavy fraction comprising the liquefaction process solvent for recycle to aid in solubilization of the coal and a third light fraction comprising the deashing solvent for recycle to aid in the production of the feed mixture.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.