Apparatus for nickel plating
US4183320A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Aug 17, 1977 |
| Grant date | Jan 15, 1980 |
| Priority date | — |
| Expiry date | Aug 17, 1997 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC23C16/45578
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
A method and apparatus for the nickel-plating of components, in which the finished component, which is to be nickel-plated, is heated to a temperature between 150.degree. and 200.degree. C. and is at the same time subjected to a continuously flowing gas stream containing nickeltetracarbonyl (Ni(CO).sub.4) and an entrainment gas. In this procedure nickel is constantly desposited from the gas phase on the heated surface from the gas stream which continuously flows around the finished component and consists of an entrainment gas and nickeltetracarbonyl. The nickel coating produced by this procedure adheres well, given normal pre-cleaning, and is practically seal-tight even in very thin coating thicknesses (0.1-1.mu.).
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.