Method of manufacturing 12 to 14% Mn steel components with weldable end pieces

US4185773A · kind A · utility

1Cited by
4References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 29, 1976
Grant dateJan 29, 1980
Priority date
Expiry dateOct 29, 1996

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB22D19/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Method of manufacturing steel components containing 12 to 14% by weight of manganese having an austenitic structure, said parts being provided with steel end pieces having a mainly austenitic structure permitting their junction by welding to components made of any desired alloy, wherein, before applying thermal treatment, said end pieces are cast into moulds disposed directly at the ends of said manganese steel components. The ends of the manganese steel component are shaped and the end pieces are subsequently cast thereon in such a manner that each end of the part comprises a front surface inclined about a transverse horizontal axis.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.