Protected iron tracer composition and method of making
US4188408A · kind A · utility
6Cited by
5References
12Claims
0Family size
Assignee
Inventor
Key dates
| Filing date | Jul 18, 1975 |
| Grant date | Feb 12, 1980 |
| Priority date | — |
| Expiry date | Jul 18, 1995 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S426/807
- WIPO fieldFood chemistry
- WIPO sectorChemistry
Abstract
Finely divided iron is mechanically mixed in water to add a coating to the iron particles. Present in the water to protect the iron from corrosion loss during such processing is a small amount of sodium carbonate or tri-sodium phosphate or sodium silicate. The inhibitor is adsorbed on the eventual iron particles after the water is driven off.