Cured aromatic polyester composition and process for its production
US4196066A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 30, 1978 |
| Grant date | Apr 1, 1980 |
| Priority date | — |
| Expiry date | Jun 30, 1998 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G63/916
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A cured or uncured linear aromatic polyester composition melt-blended and composed of PA0 (A) 100 parts by weight of a saturated linear aromatic polyester in which at least 70 mole % of the acid component consists of an aromatic dicarboxylic acid, and PA0 (B) 0.1 to 50 parts by weight of a reactive compound which is solid at room temperature or is a liquid having a boiling point of at least 200.degree. C. under atmospheric pressure, and which contains in its molecule at least one aliphatic unsaturated group substantially non-reactive with the polyester (A) and the aliphatic unsaturated group of the reactive compound (B) under conditions of melt-blending with the polyester (A) and at least one epoxy group reactive with the polyester (A) under the melt-blending conditions. The cured linear aromatic polyester composition can be prepared by extruding the uncured linear aromatic polyester composition under melting conditions, and subjecting the resulting extrudate to a curing treatment.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.