Production of non-stick coatings
US4202929A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Oct 6, 1978 |
| Grant date | May 13, 1980 |
| Priority date | — |
| Expiry date | Oct 6, 1998 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31663
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
In the production of non-adherent coated paper substrate by applying to the substrate a solvent-containing mixture comprising (A) an .alpha.,.omega.-polyorganosiloxanediol, (B) an organosiloxane containing Si-H groups, (C) an alkyl- or alkenyl-triacetoxysiloxane, (D) an organic isocyanate with more than two isocyanate radicals and (E) a hardening catalyst, and then heating the substrate to harden the coating, the improvement which comprises including in the mixture applied to the substrate a reaction product (F) of a chloromethylpolymethylsiloxane of the formula EQU ClCH.sub.2 (CH.sub.3).sub.2 Si[OSi(CH.sub.3)CH.sub.2 Cl].sub.n OSi(CH.sub.3).sub.2 Cl wherein n is from 2 - about 200, with at most an equivalent molar amount of a primary alkyl, alkenyl or cycloalkyl amine with about 4-18 carbon atoms, e.g. butylamine, hexylamine, cyclohexylamine, 2-ethylhexylamine and allylamine. The coating hardens in a very short time in a drying oven but at normal temperatures the mass has a relatively long pot life.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.