Process for improving the quality of steel sections

US4203783A · kind A · utility

5Cited by
1References
2Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 18, 1978
Grant dateMay 20, 1980
Priority date
Expiry dateSep 18, 1998

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10S148/902
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The elastic limit and breaking load of steel sections are improved by a process of surface quenching and self-tempering comprising a cooling stage followed by rapid cooling which is interrupted to allow the quenched surface layer of the section to be tempered by heat from non-quenched inner portions of the section. The rapid cooling is succeeded by a slow cooling.