Method of producing non-oriented silicon steel sheets having an excellent electromagnetic property
US4204890A · kind A · utility
38Cited by
9References
7Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Nov 8, 1978 |
| Grant date | May 27, 1980 |
| Priority date | — |
| Expiry date | Nov 8, 1998 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC21D8/1272
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Non-oriented silicon steel sheets having an excellent electromagnetic property is obtained by annealing a hot rolled steel sheet containing not moe than 0.02% of C, 0.5-3.5% of Si, 0.1-1.0% of Al, 0.1-1.0% of Mn, not more than 0.007% of S and 0.005-0.30% of Sb at a temperature of 700.degree.-950.degree. C., cold rolling the annealed sheet, and annealing the cold rolled sheet at a temperature of 750.degree.-1,000.degree. C.