Patent · US Expired

Method of stabilizing aqueous fine coal slurry and product thereof

US4208217A · kind A · utility

13Cited by
2References
24Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 25, 1978
Grant dateJun 17, 1980
Priority date
Expiry dateSep 25, 1998

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10S588/901
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

An aqueous fine coal slurry is stabilized by (a) intimately admixing the aqueous slurry containing between about 30 and about 80 percent fine coal refuse solids by weight with a stabilizing additive comprising Portland cement and (b) allowing the admixture to harden. Preferably the stabilizing additive additionally comprises finely divided blast furnace slag. Also it is preferred that sufficient additive is added so that the slurry will harden to an unconfined compressive strength of at least about 18 psi in less than about two days of addition of the additive.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.