Warp size for filament yarn consisting essentially of polyvinyl alcohol having a degree of hydrolysis of 88-100%, quaternary ammonium surfactant and plasticizer
US4222922A · kind A · utility
14Cited by
3References
10Claims
0Family size
Assignee
Inventor
Key dates
| Filing date | Dec 27, 1978 |
| Grant date | Sep 16, 1980 |
| Priority date | — |
| Expiry date | Dec 27, 1998 |
Classification
- Technology area (CPC D)Textiles; Paper
- CPC primaryD06M2200/40
- WIPO fieldTextile and paper machines
- WIPO sectorMechanical engineering
Abstract
An improved warp size for filament yarn is provided consisting essentially of polyvinyl alcohol, alkyl phenoxy (or cresoxy) ethoxyethyl dimethylbenzyl ammonium chloride and a plasticizer such as glycerol or urea, which when applied to filament yarn from aqueous solution provides excellent weaving efficiency and ease of removal combined with low shedding in the loom.